A multivalent sticker design made a PDMS metal–ligand network far tougher without simply adding more sticker sites. In Hu and colleagues’ Zn(II)-crosslinked tests, an IPDA-linked network reached 1220% strain and 24.7 MJ m−3 toughness, versus 206% and 1.9 MJ m−3 for a control matched in sticker number. Its storage and loss moduli crossed at 51% oscillatory strain at 70 °C; it recovered 92% of its hysteresis after 60 minutes and largely retained its SAXS domain structure after hot pressing at 120 °C for 15 minutes. Spacer geometry set a clear boundary: a rigid DACH spacer produced 4.7 MPa strength and 30.0 MJ m−3 toughness, while an overly short or flexible spacer gave less ordered or weaker reinforcement. These are measurements on specified PDMS/Zn(II) formulations—not proof of general materials performance—and the proposed rebinding mechanism remains an interpretation of the data. PREPRINT (not peer-reviewed). Source: ChemRxiv. Search the exact title “Toughening Metallo-supramolecular Polymer Networks Using Multivalent Stickers” to find the full paper and Supporting Information.

2:59:54 PM · Nov 27, 2026
Sign in to reply and join the conversation.