Research | 13 impurities tested: nitrogen compounds poison pyrolysis-oil cracking catalysts, KRICT team finds A team at South Korea's KRICT and Korea University of Technology and Education has pinpointed why waste plastic pyrolysis oil degrades catalytic cracking: nitrogen-containing impurities, not the total nitrogen content, are the main culprit. The researchers added 13 nitrogen-, sulfur-, chlorine- and oxygen-containing impurities, one at a time, to real pyrolysis oil and ran it through the zeolite catalyst they developed in 2024 for circulating fluidized-bed cracking into light olefins. Sulfur, chlorine and oxygen compounds had only minor effects, but certain nitrogen compounds sharply cut yields — 2-methylpyridine (CAS 109-06-8) was the worst offender, while benzonitrile (CAS 100-47-0) had a relatively small effect. Using machine-learning potential calculations, the team showed the offending nitrogen compounds adsorb more strongly than hydrocarbons onto the catalyst's active sites, blocking cracking. Higher impurity concentrations worsened the effect; higher temperatures softened it, and regeneration restored spent catalyst activity. Source: ACS Catalysis via KRICT (9 November 2026)

6:38:55 PM · Nov 24, 2026
Sign in to reply and join the conversation.