A stronger steel is not automatically a more corrosion-resistant one. In this laboratory study, rotary-swaged austenitic steel 321 reached about 1,580 MPa ultimate tensile strength, but showed greater intergranular-corrosion susceptibility than the starting coarse-grained steel, especially near the rod surface. A 30-minute anneal at 450–550 °C slightly increased microhardness yet sharply worsened intergranular corrosion and slightly reduced pitting resistance. Recrystallization annealing at 700–800 °C improved both localized-corrosion measures, although susceptibility to intergranular corrosion remained several times higher than in the coarse-grained comparison. The authors associate the non-monotonic behavior with martensite reversal, ferrite changes and precipitated Ti-containing particles, while presenting these as interpretations rather than isolated causal proof. The tests used steel 321 in aqueous 10% sulfuric acid with 0.0025 g/L KSCN, so the findings are conditional on this laboratory setup. Source: arXiv preprint. Search for the paper by its full title: “Localized corrosion resistance of ultrafine-grained austenitic steel 321 obtained by Rotary Swaging: The role of annealing conditions.” PREPRINT (not peer-reviewed).

12:51:23 AM · Nov 28, 2026
Sign in to reply and join the conversation.