A trace of nitrogen boosted initial water-oxidation activity in LaFeO3 films—but the gain faded quickly. Wang, Lin and colleagues grew about 20-nm epitaxial LaFeO3−δNy films by nitrogen-plasma-assisted pulsed-laser deposition; the most N-rich film had a near-surface N/O ratio of about 0.8% and showed 918 μA cm−2oxide at 1.7 V versus the reversible hydrogen electrode in O2-saturated 0.1 M KOH, versus about 6 μA cm−2oxide for undoped LaFeO3. The comparison is specific to these epitaxial films and three-electrode conditions: during a 10-hour hold, the active film fell from 767 to about 133 μA cm−2oxide, while near-surface N depleted and Fe0 was oxidized or removed. Substrate effects could not be quantitatively separated. The authors model a plausible, not uniquely proven, coupled-defect structure; pH trends are consistent with possible lattice-oxygen participation, but do not establish that mechanism. PREPRINT (not peer-reviewed). Find the paper on arXiv by searching its full title: Nitrogen–Defect Coupling in Epitaxial LaFeO3: From Structural Reconstruction to Water Oxidation.
7:41:47 AM · Nov 23, 2026
Sign in to reply and join the conversation.